Aluminum ash corrosion resistance of alumina-silica refractory castables
Dong Yuchen, Zhang Sanhua, Qin Hongbin, Li Pengxin, Cao Yingnan
Refractories . 2025, (5): 422 -426 .  DOI: 10.3969/j.issn.1001-1935.2025.05.009