Synthesis of SiAlON composite powders by carbothermal reduction and nitridation of coal gasification slag
Guo Shimeng, Yin Hongfeng, Jia Huan, Xin Yalou, Tang Yun, Yuan Hudie, Ren Xiaohu
Refractories . 2025, (
6
): 466 -470 . DOI: 10.3969/j.issn.1001-1935.2025.06.002