Effects of recycled Al 2O 3-C composite slide gate material addition on properties of Al 2O 3-SiC-C castables
Chen Cong, Han Bingqiang, Wei Jiawei, Zhong Hutang, Zhao Haohao, Duan Junlong
Refractories . 2025, (6): 471 -476 .  DOI: 10.3969/j.issn.1001-1935.2025.06.003