Preparation of SiO 2-coated MgO composite powders by sol-gel method and their properties
Zhou Zhang-yan, Cao Jiyuan, Ma Beiyue, Li Guangming, Song Na, Ban Xia, Liu Yongli, Zhang Chengcheng, Zhao Guang-yi
Refractories . 2025, (6): 488 -494 .  DOI: 10.3969/j.issn.1001-1935.2025.06.006