Effect of fused magnesia on properties of anorthite-spinel insulation refractories
Wang Shizhen, Han Bing-qiang, Tan Dan, Wei Yaowu, Yan Wen, Li Nan
Refractories . 2026, (1): 1 -7 .  DOI: 10.3969/j.issn.1001-1935.2026.01.001