Micro-nano pore control and properties of thermal insulation carbon fiber composites
Chen Jialiang, Ding Jun, Luo Yixin, Liu Zhenglong, Yu Chao, Zhu Qingyou, Deng Chengji
Refractories . 2026, (
1
): 48 -53 . DOI: 10.3969/j.issn.1001-1935.2026.01.009