Preparation of Al-Si alloy phase change thermal storage composite ceramics by selective laser sintering and their strengthening and toughening mechanism
Li Yinfei, Zhang Meijie, Gu Huazhi, Chen Ling, Yang Shuang, Huang Ao, Yin Yucheng
Refractories . 2026, (2): 124 -130 .  DOI: 10.3969/j.issn.1001-1935.2026.02.007