Effect of La(OH)
3
on properties of MgO-bonded corundum castables
Tang Yaping, Bi Wenjian, Zhang Hong-rui, Yang Zhisen, Zeng Zhihao, Li Fen, Chen Liugang
Refractories . 2026, (
4
): 295 -299 . DOI: 10.3969/j.issn.1001-1935.2026.04.004