Effect of carbon nanofiber/calcium aluminate composite powder on properties of ceramic composite resistors
Zhong Zhenxin, Yao Congwei, Wang Yunlong, Zhu Ruifeng, Wang Jiayi, Chong Xiaochuan, Xiao Guoqing, Ding Donghai
Refractories . 2026, (
5
): 415 -421 . DOI: 10.3969/j.issn.1001-1935.2026.05.008