Research progress of application of additives in MgO-MA materials
Zhang Yucui, Cui Qingyang, Gao Song, Jiao Zhiyu, Hu Yancang
Refractories . 2021, (1): 89 -92 .  DOI: 10.3969/j.issn.1001-1935.2021.01.019