催化氮化制备氮化硅研究进展

王鑫1), 王军凯1), 黄珍霞2), 孟浩1), 王一菲1), 温研科1)   

  1. 1)河南理工大学 材料科学与工程学院 河南焦作 454003
    2)河南理工大学 化学化工学院 河南焦作 454003
  • 收稿日期:2022-06-23 出版日期:2023-06-15 发布日期:2023-06-21
  • 通讯作者: 王军凯,男,1988年生,博士,讲师。E-mail:jkwang@hpu.edu.cn
  • 作者简介:王鑫:男,1999年生,硕士研究生。E-mail:2855935831@qq.com
  • 基金资助:
    国家自然科学基金资助项目(52102017);河南省科技攻关计划资助项目(212102210589);河南省博士后项目启动资助项目(2020SZZ02);河南理工大学博士基金项目(B2019-40);河南省高校基本科研业务费专项资金资助项目(NSFRF220410)。

Research progress on preparation of silicon nitride by catalytic nitridation

Wang Xin, Wang Junkai, Huang Zhen-xia, Meng Hao, Wang Yifei, Wen Yanke   

  1. First author’s address: School of Materials Science and Engineering, Henan Polytechnic University, Jiaozuo 454003, Henan, China
  • Received:2022-06-23 Online:2023-06-15 Published:2023-06-21

摘要: 氮化硅具有高强度、耐高温、耐腐蚀耐磨损、抗热震、抗氧化等优良性能,被广泛应用于耐火材料、冶金及航天等领域。催化氮化法是在硅粉氮化过程中引入催化剂,不仅能够实现硅粉的低温快速氮化,而且能够改变产物的形貌,促进氮化硅晶须的生成,进而改善制品的显微结构,提高其力学性能。为此,综述了金属单质和金属氧化物作为催化剂催化氮化制备氮化硅的研究进展,并展望了催化氮化制备氮化硅工艺今后的发展方向。

关键词: 氮化硅, 催化氮化, 金属单质, 金属氧化物, 催化机制

Abstract: Silicon nitride is widely used in refractories,metallurgy,aerospace and other fields due to its excellent properties,such as high strength and good resistance to high-temperature,corrosion,wear,thermal shock and oxidation.The introduction of catalyst into the nitriding process of silicon powder by the catalytic nitriding method can not only realize the rapid nitriding of silicon powder at low temperatures,but also change the morphology of the products,promote the formation of silicon nitride whiskers,improve the microstructure of the products,and enhance the mechanical properties.The research progress on the preparation of silicon nitride by catalytic nitriding with metals and metallic oxides as catalysts was reviewed,and the future development direction was prospected.

Key words: silicon nitride, catalytic nitriding, metal, metallic oxide, catalytic mechanism