二茂铁含量对不烧镁钙系耐火材料性能的影响

李金锋1)(), 王黎1,2,3)(), 漆小鹏1), 钟俊鹏2), 张宇2), 张敦新4)   

  1. 1)江西理工大学 江西赣州 341000
    2)洛阳理工学院 河南洛阳 471000
    3)洛阳市科创绿色建材研究院 河南洛阳 471000
    4)山东鲁桥新材料股份有限公司 山东淄博 255200
  • 收稿日期:2020-06-01 出版日期:2021-02-15 发布日期:2021-02-15
  • 通讯作者: 王黎,男,1968年生,博士,副教授。E-mail: Wangli6433@sina.com
    王黎,男,1968年生,博士,副教授。E-mail: Wangli6433@sina.com
  • 作者简介:李金锋:男,1992年生,硕士研究生。E-mail: 948328160@qq.com
  • 基金资助:
    河南省高新技术领域科技攻关项目(152102210122)

Effect of ferrocene content on properties of unburned magnesia-calcia refractories

Li Jinfeng1)(), Wang Li1,2,3)(), Qi Xiaopeng1), Zhong Junpeng2), Zhang Yu2), Zhang Dunxin4)   

  1. 1)Jiangxi University of Science and Technology,Ganzhou 341000,Jiangxi,China
  • Received:2020-06-01 Online:2021-02-15 Published:2021-02-15
  • Contact: Wang Li

摘要:

以人工合成镁钙砂、电熔镁砂为主原料,无水酚醛树脂作为结合剂,制备了不烧镁钙系试样。研究了二茂铁外加量(质量分数分别为0、0.5%、1%、1.5%)对试样性能的影响,并通过SEM和XRD分析了试样的显微结构和相组成。结果表明:1)经过200、1 650 ℃热处理后,试样的体积密度、常温耐压强度和抗水化时长随着二茂铁含量的增加呈先上升后下降的趋势,当二茂铁含量为1%(w)时,性能最佳;2)1 650 ℃热处理后,二茂铁的引入可以在试样中形成铁酸钙,且有部分碳残留。

关键词: 二茂铁, 镁钙砂, 不烧镁钙砖, 显微结构, 抗水化

Abstract:

Unburned magnesia-calcium based specimens were prepared using synthetic magnesia-calcia sand and fused magnesia as the main raw materials,anhydrous phenolic resin as the binder.Effect of the ferrocene addition (0,0.5%,1%,and 1.5%,by mass) on the specimens was researched.SEM and XRD were used to characterize the microstructure and phase composition of the specimens.The results show that:(1)the bulk density,the cold crushing strength and the hydration resistance of the specimens increase first and then decrease as the ferrocene addition increases after heat treatment at 200 ℃ and 1 650 ℃;when the ferrocene addition is 1%,the performance of the specimens is the best;(2)the introduction of ferrocene can form calcium ferrite in the specimen and some carbon remains after the heat treatment at 1 650 ℃.

Key words: ferrocene, magnesia-calcium sand, unburned magnesia-calcia brick, microstructure, hydration resistance