耐火材料 ›› 2021, Vol. 55 ›› Issue (6): 502-504.DOI: 10.3969/j.issn.1001-1935.2021.06.009

• 研究开发 • 上一篇    下一篇

煅烧温度对莫来石质多孔陶瓷材料性能的影响

胡其国(), 王明华, 邵晴, 李济, 李小龙   

  1. 江西陶瓷工艺美术职业技术学院 江西景德镇 333001
  • 收稿日期:2021-01-15 出版日期:2021-12-15 发布日期:2021-12-10
  • 作者简介:胡其国:男,1988年生,博士。 E-mail: 461044339@qq.com
  • 基金资助:
    江西省教育厅科技重点项目(GJJ204301)

Effect of calcination temperature on properties of porous mullite ceramic materials

Hu Qiguo(), Wang Minghua, Shao Qing, Li Ji, Li Xiaolong   

  1. Jiangxi Arts & Ceramics Technology Institute,Jingdezhen 333001,Jiangxi,China
  • Received:2021-01-15 Online:2021-12-15 Published:2021-12-10

摘要:

为了粉煤灰漂珠的高附加值利用,以粉煤灰漂珠为模板,铝矾土为铝源,AlF3和V2O5为添加剂,采用黏附法与固相烧结技术制备了莫来石质多孔陶瓷材料,研究了煅烧温度(分别为1 100、1 200、1 300和1 350 ℃)对莫来石质多孔陶瓷材料物相组成、显微形貌和性能的影响。结果表明:1)随着煅烧温度从1 100 ℃升高至 1 350 ℃,试样中莫来石的衍射峰逐渐增强,石英衍射峰逐渐减弱直至消失;2)随着煅烧温度从1 100 ℃升高至1 350 ℃,试样的显气孔率先增大后减少,体积密度和耐压强度先减少后增大;3)当煅烧温度为1 300 ℃时,试样的显气孔率为68.4%,体积密度为0.72 g·cm-3,耐压强度为14.6 MPa。

关键词: 煅烧温度, 粉煤灰漂珠, 多孔莫来石, 铝矾土, 显微结构

Abstract:

For improve the high value-added utilization of fly ash floater,porous mullite ceramic materials were prepared by adhesion method and solid-phase sintering using fly ash floater as the template,bauxite as the aluminum source,AlF3 and V2O5 as the additives.Effects of the calcination temperature (1 100,1 200,1 300,and 1 350 ℃,respectively) on the phase composition,the microstructure and the properties of the prepared materials were studied.The results show that: when the temperature changes from 1 100 ℃ to 1 350 ℃,the diffraction peaks of the mullite gradually increase,and these of the quartz gradually weaken until disappear,the apparent porosity of the specimens increases firstly and then decreases,while the bulk density and the compressive strength are on the contrary;when the calcination temperature is 1 300 ℃,the specimen has the apparent porosity of 68.4%,the bulk density of 0.72 g·cm-3,and the compressive strength of 14.6 MPa.

Key words: calcination temperature, fly ash floater, porous mullite, bauxite, microstructure