[1] LIU M,YANG Y,WEI Y Q,et al.Preparation of dense and high-purity SiC ceramics by pressureless solid-state-sintering[J].Ceramics International,2019,45(16):19771-19776. [2] 杨千秋,董博,余超,等.SiCf对重结晶碳化硅陶瓷的烧结颈结构作用机制[J].陶瓷学报,2023,44(2):289-295. [3] 马北越,刘健,李定勇.造孔剂对SiC多孔陶瓷材料性能的影响[J].耐火材料,2020,54(4):310-313. [4] ZHANG Z J,WEI Z L,LI Z Y,et al.SiC honeycomb reinforced Al matrix composite with improved tribological performance[J].Ceramics International,2021,47(16):23376-23385. [5] XU M,GIRISH Y R,RAKESH K P,et al.Recent advances and challenges in silicon carbide(SiC)ceramic nanoarchitectures and their applications[J].Materials Today Communications,2021,28:102533. [6] 洪智亮,张巧君,李开元,等.SiC/SiC复合材料在高温空气中的氧化行为[J].材料工程,2021,49(5):144-150. [7] WANG Y C,LIU H Y,MEI D Q,et al.A novel thermally autonomous methanol steam reforming microreactor using SiC honeycomb ceramic as catalyst support for hydrogen production[J].International Journal of Hydrogen Energy,2021,46(51):25878-25892. [8] SUNG H W,LEE G W,YUN E S,et al.Novel process for recrystallized silicon carbide through β-α phase transformation[J].Ceramics International,2020,46(14):21920-21924. [9] 梁宇恒,朱时珍,王扬卫,等.浆料固含量和颗粒配比对重结晶烧结SiC的影响[J].稀有金属材料与工程,2015(S1):524-527. [10] 李小池,王涛.重结晶碳化硅制品等静压成型研究[J].西安科技大学学报,2014,34(3):345-349. [11] 梁鹏鹏,吴吉光,陈红伟,等.重结晶SiC陶瓷支撑体的制备及性能[J].耐火材料,2018,52(6):442-445. [12] 邢广超.不同气氛下Al4SiC4对重结晶碳化硅微观结构与性能的影响[D].武汉:武汉科技大学,2020. [13] 李晓池,刘明刚,朱海马.烧结助剂对重结晶SiC电热元件性能的影响[J].西安科技大学学报,2010,30(2):217-221. [14] 董博,余超,邓承继,等.碳化硅陶瓷导热性能的研究进展[J].材料工程,2023,51(1):64-75. [15] 黄进,吴昊天,万龙刚.重结晶碳化硅材料的制备与应用研究进展[J].耐火材料,2017,51(1):73-77. [16] 邢媛媛,吴海波,刘学建,等.颗粒级配对固相烧结碳化硅陶瓷的影响[J].无机材料学报,2018,33(11):1167-1172. [17] 关梦珂,徐慢,王树林,等.颗粒级配对碳化硅陶瓷膜性能的影响[J].建材世界,2021,42(2):6-9. [18] GUO W M,XIAO H N,LIU J X,et al.Effects of B4C on the microstructure and phase transformation of porous SiC ceramics[J].Ceramics International,2015,41(9A):11117-11124. [19] LI Y J,WU H B,LIU X J,et al.Microstructures and properties of porous liquid-phase-sintered SiC ceramic by hot press sintering[J].Materials,2019,12(4):639. [20] 周健儿,杨玉龙,常启兵,等.颗粒级配对氧化铝多孔陶瓷膜支撑体孔径及抗折强度的影响[J].人工晶体学报,2014,43(8):2125-2131. [21] 申轶男,陈华辉,胡宇.原料颗粒级配对多孔陶瓷性能的影响[J].材料研究学报,2011,25(5):550-556. [22] 李君,员文杰,邓承继,等.SiC原料颗粒级配对Si3N4结合SiC复合陶瓷材料的影响[J].中国陶瓷工业,2012,19(6):9-13. [23] 何江锋,张海军,葛胜涛,等.SiC多孔陶瓷制备方法研究进展[J].耐火材料,2020,54(2):163-171. [24] APETZ R,VAN BRUGGEN M P B.Transparent alumina:a light-scattering model[J].Journal of the American Ceramic Society,2003,86(3):480-486. [25] 董博,余超,邓承继,等.反应烧结碳化硅高温性能的研究进展[J].耐火材料,2022,56(1):75-81. [26] 董博,邓承继,余超,等.烧成温度对反应烧结碳化硅蜂窝陶瓷的性能调控[J].陶瓷学报,2023,44(1):89-94. [27] 余超,邢广超,吴郑敏,等.亚微米Al2O3对重结晶碳化硅的作用机制[J].材料研究学报,2022,36(9):679-686. |