耐火材料 ›› 2025, Vol. 59 ›› Issue (6): 511-515.DOI: 10.3969/j.issn.1001-1935.2025.06.010

• 研究开发 • 上一篇    下一篇

热处理温度对高熵尖晶石涂层性能的影响

孙帅蒙, 杨爽, 张美杰, 付绿平, 黄奥, 顾华志   

  1. 武汉科技大学 先进耐火材料全国重点实验室 湖北武汉 430081
  • 收稿日期:2025-02-05 出版日期:2025-12-15 发布日期:2025-12-23
  • 通讯作者: 杨爽,男,1987年生,博士,副教授。E-mail:shuang_yang@wust.edu.cn
  • 作者简介:孙帅蒙:男,1998年生,硕士研究生。E-mail:2869989240@qq.com
  • 基金资助:
    国家自然科学基金面上资助项目(52172023,52272022);湖北省自然科学基金杰出青年项目(2021CFA071)。

Effect of heat treatment temperature on properties of high-entropy spinel coatings

Sun Shuaimeng, Yang Shuang, Zhang Meijie, Fu Lyuping, Huang Ao, Gu Huazhi   

  1. First author’s address:State Key Laboratory of Advanced Refractories,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2025-02-05 Online:2025-12-15 Published:2025-12-23

摘要: 为拓展高熵尖晶石红外辐射涂层在节能减排领域的应用,首先以氧化镁、氧化铝、氧化钴、氧化镍、氧化铜、氧化锌为原料,按1∶5∶1∶1∶1∶1的化学计量比混合,经1 600 ℃热处理8 h制备高熵尖晶石。然后在30 mm×30 mm×10 mm的刚玉-莫来石小试块表面喷涂高熵尖晶石红外辐射涂层。探究不同热处理温度(1 300、1 400、1 500和1 600 ℃保温2 h)对该涂层的红外辐射性能和结合强度的影响。结果发现:热处理温度由1 300 ℃提高至1 600 ℃时,涂层的孔隙逐渐减少,结构逐渐致密;涂层经1 600 ℃保温2 h后室温下0.2~2.5 μm波段和2.5~15 μm波段的红外发射率分别达到0.86和0.90;当热处理温度为1 500 ℃时,涂层与基体的结合强度最高,达到6.16 MPa。

关键词: 高熵尖晶石, 红外辐射涂层, 热处理温度, 发射率, 结合强度

Abstract: To expand the application of high-entropy spinel infrared radiation coatings in the field of energy saving and emission reduction,high-entropy spinel was prepared by heat treatment at 1 600 ℃ for 8 h with magnesia,alumina,cobalt oxide,nickel oxide,copper oxide and zinc oxide as raw materials,mixed in a stoichiometric ratio of 1∶5∶1∶1∶1∶1.Then it was sprayed on the surface of corundum-mullite small test blocks of 30 mm×30 mm×10 mm to form a high-entropy spinel infrared radiation coating.The effects of different heat treatment temperatures (1 300,1 400,1 500 and 1 600 ℃ for 2 h) on the infrared radiation performance and bonding strength of the coating were investigated.It is found that as the temperature increases from 1 300 to 1 600 ℃,the pores of the coating are gradually reduced,leading to a denser structure.The coating heat treated at 1 600 ℃ for 2 h has the infrared emissivity of 0.86 in the 0.2-2.5 μm band and 0.90 in the 2.5-15 μm band at room temperature.After the heat treatment at 1 500 ℃,the bonding strength between the coating and the substrate is the highest,6.16 MPa.

Key words: high-entropy spinel, infrared radiation coatings, heat treatment temperature, emissivity, bonding strength