炉排式生活垃圾焚烧炉用耐火砖砖型设计标准化研究
王峰裕, 占华生, 张体强, 蒋自兴, 肖大勇, 王天帅, 袁真强, 邓信开, 张海元, 高长贺
Standardization research of refractory brick type design for household refuse grate incinerators
Wang Fengyu, Zhan Huasheng, Zhang Tiqiang, Jiang Zixing, Xiao Dayong, Wang Tianshuai, Yuan Zhen-qiang, Deng Xinkai, Zhang Haiyuan, Gao Changhe
耐火材料 . 2021, (2): 155 -160 .  DOI: 10.3969/j.issn.1001-1935.2021.02.015