“一包到底”铁水包漏铁事故分析及对策
王凯, 鲁俭, 魏继东, 李宏伟
Analysis and countermeasures of ladle iron leakage accident of “one ladle to the end”
Wang Kai, Lu Jian, Wei Jidong, Li Hongwei
耐火材料 . 2021, (3): 240 -243 .  DOI: 10.3969/j.issn.1001-1935.2021.03.014