锆英石碳热还原制备ZrB
2-ZrO
2-SiC复合粉体
周超杰, 张磊, 赵飞, 贾全利, 刘新红, 钟香崇
Preparation of ZrB
2-ZrO
2-SiC composite powder using zircon by carbothermal reduction method
Zhou Chao-jie, Zhang Lei, Zhao Fei, Jia Quanli, Liu Xinhong, Zhong Xiangchong
耐火材料
.
2022, (1): 20
-23
.
DOI: 10.3969/j.issn.1001-1935.2022.01.005