煅烧制度对微晶菱镁矿制备高致密度烧结镁砂性能的影响
田晓利, 李志勋, 冯润棠, 张洁, 郑全福, 史旭武, 杜永彬
Effect of calcination schedule on properties of high density sintered magnesia prepared from microcrystalline magnesite
Tian Xiaoli, Li Zhixun, Feng Runtang, Zhang Jie, Zheng Quanfu, Shi Xuwu, Du Yongbin
耐火材料 . 2022, (5): 400 -406 .  DOI: 10.3969/j.issn.1001-1935.2022.05.007