硅溶胶改性多层石墨烯的润湿性研究
郁柏松, 朱业宁, 李炀哲, 苏玉庆, 魏军从, 涂军波, 王义龙
Wettability of silica sol modified multilayer graphene
Yu Baisong, Zhu Yening, Li Yangzhe, Su Yuqing, Wei Juncong, Tu Junbo, Wang Yilong
耐火材料
.
2022, (6): 523
-526
.
DOI: 10.3969/j.issn.1001-1935.2022.06.014