天然菱镁矿对转炉环保型水基镁质修补料性能的影响
戴晨晨, 聂波华, 张万普, 黄宇, 卢杨, 赫丽杰
Effect of natural magnesite on properties of environment-friendly water-based magnesia repair mixes for converters
Dai Chenchen, Nie Bohua, Zhang Wanpu, Huang Yu, Lu Yang, He Lijie
耐火材料 . 2022, (6): 530 -534 .  DOI: 10.3969/j.issn.1001-1935.2022.06.016