烧结温度对莫来石多孔陶瓷结构与性能的影响
郭会师, 陈文亮, 李文凤, 杨佳麟, 秦笑梅, 桂阳海, 刘应凡
Effects of sintering temperatures on microstructure and properties of mullite porous ceramics
Guo Huishi, Chen Wenliang, Li Wenfeng, Yang Jialin, Qin Xiaomei, Gui Yanghai, Liu Yingfan
耐火材料 . 2023, (1): 10 -14 .  DOI: 10.3969/j.issn.1001-1935.2023.01.003