耐火材料 ›› 2023, Vol. 57 ›› Issue (1): 10-14.DOI: 10.3969/j.issn.1001-1935.2023.01.003

• 研究开发 • 上一篇    下一篇

烧结温度对莫来石多孔陶瓷结构与性能的影响

郭会师1), 陈文亮1), 李文凤2), 杨佳麟1), 秦笑梅1), 桂阳海1), 刘应凡1)   

  1. 1)郑州轻工业大学 材料与化学工程学院 河南郑州 450001
    2)河南工业大学 材料科学与工程学院 河南郑州 450001
  • 收稿日期:2022-05-19 出版日期:2023-02-15 发布日期:2023-02-21
  • 作者简介:郭会师:男,1984年生,博士,讲师。E-mail:guohuishi@zzuli.edu.cn
  • 基金资助:
    国家自然科学基金资助项目(51802290,U1904213,U20041102);河南省重点科技攻关项目(182102210613,202102210260,172102210223)。

Effects of sintering temperatures on microstructure and properties of mullite porous ceramics

Guo Huishi, Chen Wenliang, Li Wenfeng, Yang Jialin, Qin Xiaomei, Gui Yanghai, Liu Yingfan   

  1. School of Material and Chemical Engineering,Zhengzhou University of Light Industry,Zhengzhou 450001,Henan,China
  • Received:2022-05-19 Online:2023-02-15 Published:2023-02-21

摘要: 以含锆硅线石为主要原料,α-Al2O3粉为辅料,改性淀粉为造孔剂,原位烧结制备了莫来石多孔陶瓷试样。研究了烧结温度(1 400~1 600 ℃,间隔50 ℃)对试样物相组成、显微结构及性能的影响。结果表明:1)随烧结温度的升高,试样中莫来石衍射峰的强度逐渐增强,莫来石晶粒逐渐发育长大,其外观呈现明显的台阶状形貌,符合二维成核生长机制。2)随烧结温度的升高,烧后试样的体积密度呈先减后增趋势,而显气孔率和线变化率的变化趋势则与之相反,常温耐压强度则呈逐渐增大趋势。3)当烧结温度为1 550~1 600 ℃时,试样综合性能较佳,莫来石晶粒发育长大并致密结合,适于在高温下使用。

关键词: 硅线石, 莫来石, 多孔陶瓷, 烧结温度, 生长机制

Abstract: Mullite porous ceramics were prepared by in-situ sintering using zirconia-containing sillimanite as the main raw material,α-Al2O3 powder as the auxiliary material and modified starch as the pore-forming agent.The effects of the sintering temperature (1 400-1 600 ℃,an interval of 50 ℃) on the phase composition,the microstructure and the properties of the samples were studied.The results show that:(1)with the increase of the sintering temperature,the intensity of the mullite diffraction peaks increases and the mullite crystals gradually grow up;moreover,steps are observed on mullite surfaces,indicating that the mullite grows by two-dimensional nucleation mechanism;(2)with the increase of the sintering temperature,the bulk density of the samples decreases firstly and then increases,while the apparent porosity and the linear change show the opposite trends,but the cold compressive strength increases gradually;(3)when the sintering temperature is 1 550-1 600 ℃,the samples show the optimal comprehensive properties;mullite crystals grow up and combine closely,which makes mullite porous ceramics suitable for application at high temperatures.

Key words: sillimanite, mullite, porous ceramic, sintering temperature, growth mechanism

中图分类号: