南钢鱼雷罐炉衬保温优化及应用
李权辉, 刘桂丽, 马渭奎, 李翔, 杨文刚, 刘国齐
Thermal insulation optimization and application of torpedo ladle lining in Nanjing Iron & Steel
Li Quanhui, Liu Guili, Ma Weikui, Li Xiang, Yang Wengang, Liu Guoqi
耐火材料
.
2023, (1): 74
-77
.
DOI: 10.3969/j.issn.1001-1935.2023.01.016