莫来石晶须的制备、生长机制及应用研究进展
刘朝阳, 潘松阳, 董泽明, 文俊, 王骏阳, 于景坤
Progress in preparation,growth mechanism,and application of mullite whiskers
Liu Zhaoyang, Pan Song-yang, Dong Zeming, Wen Jun, Wang Junyang, Yu Jingkun
耐火材料
.
2023, (3): 270
-276
.
DOI: 10.3969/j.issn.1001-1935.2023.03.018