以微孔刚玉-尖晶石骨料替代刚玉骨料制备刚玉-尖晶石浇注料
刘学新, 张锦化, 陈鑫铭, 王景然, 杨宗源, 韩兵强, 柯昌明
Preparation of corundum-spinel castables using microporous corundum-spinel aggregates to replace corundum aggregates
Liu Xuexin, Zhang Jinhua, Chen Xinming, Wang Jingran, Yang Zongyuan, Han Bingqiang, Ke Changming
耐火材料
.
2023, (6): 514
-517
.
DOI: 10.3969/j.issn.1001-1935.2023.06.011