Al 2O 3-SiC-C质炮泥侵蚀过程热力学计算及抗渣性分析
鞠茂奇, 肖扬武, 夏昌勇, 梁永和, 丛培源, 魏建修, 蔡玮, 陈金凤
Thermodynamic calculation and slag resistance analysis of Al 2O 3-SiC-C taphole clay during corrosion
Ju Maoqi, Xiao Yangwu, Xia Changyong, Liang Yonghe, Cong Peiyuan, Wei Jianxiu, Cai Wei, Chen Jinfeng
耐火材料 . 2024, (2): 143 -147 .  DOI: 10.3969/j.issn.1001-1935.2024.02.010