尖晶石加入量对刚玉-尖晶石浇注料显微结构和性能的影响
薛军柱, 刘光平, 陈俊峰, 魏国平, 程亚苹, 鄢文, 李楠
Influence of spinel addition on microstructure and properties of corundum-spinel castables
Xue Junzhu, Liu Guangping, Chen Junfeng, Wei Guoping, Cheng Yaping, Yan Wen, Li Nan
耐火材料 . 2025, (2): 155 -161 .  DOI: 10.3969/j.issn.1001-1935.2025.02.012