废高铝球粉对莫来石-氧化铝-石英复相材料性能的影响
吕振飞, 范梦可, 曹钰坤, 李熹虎, 柯洋慧, 张学佳, 王学凯, 沈秀琳, 张晓光
Effects of waste high alumina sphere powder on performance of mullite-alumina-quartz multiphase materials
Lyu Zhenfei, Fan Mengke, Cao Yukun, Li Xihu, Ke Yanghui, Zhang Xuejia, Wang Xuekai, Shen Xiulin, Zhang Xiaoguang
耐火材料 . 2025, (4): 323 -329 .  DOI: 10.3969/j.issn.1001-1935.2025.04.009