真空感应熔炼高温合金与坩埚耐火材料相互作用的研究进展
刘星立, 邢一丹, 黄潇阳, 庞百胜, 黄亮, 张海军
Research progress on interaction between high-temperature alloys and crucible refractory materials during vacuum induction melting
Liu Xingli, Xing Yidan, Huang Xiaoyang, Pang Baisheng, Huang Liang, Zhang Haijun
耐火材料
.
2025, (6): 536
-541
.
DOI: 10.3969/j.issn.1001-1935.2025.06.015