Refractories ›› 2021, Vol. 55 ›› Issue (6): 539-544.DOI: 10.3969/j.issn.1001-1935.2021.06.018

Previous Articles     Next Articles

Optimization and research progress on bonding systems of refractory castables

Zhang Yanli1)(), Wang Di2), Li Ying2), Jia Quanli3)   

  1. 1) Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2020-12-15 Online:2021-12-15 Published:2021-12-10

耐火浇注料结合体系的优化与研究进展

张艳利1)(), 汪涤2), 李莹2), 贾全利3)   

  1. 1)中钢集团洛阳耐火材料研究院有限公司 河南洛阳 471039
    2)河南建筑材料研究设计院有限责任公司 河南郑州 450002
    3)郑州大学 高温材料研究所 河南郑州 450052
  • 作者简介:张艳利:女,1982年生,硕士,高级工程师。E-mail: smile8200@163.com

Abstract:

The classification of bonding systems and bonding modes of refractory castables was introduced.The research progress on new-type cements of the cement bonding system was expounded in detail.The characteristics and the application progress of sol (gel),hydration alumina,magnesia binders,phosphate (phosphoric acid),other binders that can replace cement,and new additives were illuminated.It was pointed out that the new-type cement has good application effect,but it is of high cost.The non-cement bonded castables are not easy to construct,but they are easy to bake,which is suitable for gunning mixes and precast products.The new additives greatly improve the placing performance of castables and have a broad application prospect.

Key words: refractory castables, bonding systems, new-type additives

摘要:

介绍了耐火浇注料结合体系及结合方式的主要类型,详细阐述了水泥结合体系中新型水泥的研究进展,论述了非水泥结合体系中溶胶(凝胶)、水合氧化铝、镁质结合剂、磷酸盐(磷酸)、可替代水泥的其他结合剂以及新型外加剂的性能特点与应用进展。指出新型水泥具有良好的应用效果,但新型水泥存在成本高的问题;非水泥结合剂存在施工难的问题,但易于烘烤,适用于喷补料、预制件;新型外加剂大幅改善了耐火浇注料的施工性能,具有广阔的应用前景。

关键词: 耐火浇注料, 结合体系, 新型外加剂