Refractories ›› 2022, Vol. 56 ›› Issue (2): 123-126.DOI: 10.3969/j.issn.1001-1935.2022.02.006

Previous Articles     Next Articles

Effect of binder types on properties of lanthanum aluminate coating materials

Zhang Yifan(), Wang Qu, Wang Gang(), Liu Pengcheng, Zhang Qi, Si Yaochen   

  1. State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2021-08-17 Online:2022-04-15 Published:2022-04-21
  • Contact: Wang Gang

黏结剂种类对铝酸镧涂层材料性能的影响

张一帆(), 王曲, 王刚(), 刘鹏程, 张琪, 司瑶晨   

  1. 中钢集团洛阳耐火材料研究院有限公司 先进耐火材料国家重点实验室 河南洛阳 471039
  • 通讯作者: 王刚
  • 作者简介:张一帆:女,1994年生,硕士研究生。E-mail: lirrzyf@126.com
  • 基金资助:
    国家自然科学基金联合基金资助项目(U1904217);中原科技创新领导人才项目(224200510006)

Abstract:

Lanthanum aluminate coating materials were prepared using Ca2+-Fe3+ doped lanthanum aluminate as the radiation powder matrix,aluminum dihydrogen phosphate,sodium silicate,silica sol and alumina sol as binders.The developed coating materials were spread on the surface of corundum bubble bricks,and the influences of different binders on the phase composition,the microstructure and the performance of the coating materials were explored.The results show that the coating material using alumina sol contains less impurities,which is the best binder choice.The Ca2+-Fe3+ doped lanthanum aluminate radiation agent with alumina sol as the binder performs excellent spalling resistance on the surface of the corundum bubble bricks.

Key words: lanthanum aluminate, binder, alumina sol, energy saving

摘要:

采用Ca2+-Fe3+掺杂的铝酸镧为辐射粉体基料,分别以磷酸二氢铝、水玻璃、硅溶胶和铝溶胶为黏结剂制备了铝酸镧涂层材料,将其涂覆于刚玉空心球砖表面,研究了黏结剂种类对涂层材料的物相组成、显微结构和性能的影响。结果表明:以铝溶胶为黏结剂所制得涂层杂质相对较少,为最佳的黏结剂选择;以铝溶胶为黏结剂的钙铁掺杂铝酸镧辐射剂在刚玉空心球砖表面的抗剥落性最好。

关键词: 铝酸镧, 黏结剂, 铝溶胶, 节能