Refractories ›› 2022, Vol. 56 ›› Issue (2): 170-173.DOI: 10.3969/j.issn.1001-1935.2022.02.017

Previous Articles     Next Articles

Development and application of new wear-resistant bricks for cooling zone of dry quenching coke ovens

Yan Tao1)(), Xu Guotao2), Sheng Junbo3), Wang Dachun3), Wang Xibo1), Qin Jiantao1), Xu Kun1), Wang Yuanchao1)   

  1. 1)Lunai Kiln Refractories Co.,Ltd.of Shandong Refractories Group,Zibo 255200,Shandong,China
  • Received:2021-08-22 Online:2022-04-15 Published:2022-04-21

干熄焦炉冷却段用新型耐磨砖的研制与应用

闫涛1)(), 徐国涛2), 盛军波3), 王大春3), 王希波1), 秦建涛1), 许堃1), 王远超1)   

  1. 1)山东耐材集团鲁耐窑业有限公司 山东淄博 255200
    2)宝钢股份中央研究院 湖北武汉 430080
    3)武汉平煤武钢联合焦化公司 湖北武汉 430080

Abstract:

To improve the service life of wear-resistant bricks for the cooling zone of dry quenching coke ovens,a newly wear-resistant brick was developed by adjusting the aggregates particle size distribution and adding SiC powder and andalusite micropowder on the basis of grade B mullie brick.Its practical application in a 140 t·h-1 dry quenching coke oven was introduced.The results show that the newly wear-resistant brick has the compressive strength of 160 MPa and the wear amount of only 1.92 cm3,which is better than the original grade B mullite brick.After 7 years of service in the cooling zone of a 140 t·h-1 dry quenching coke oven,the lining still shows smooth surface with slight wear and is expected to serve for more than 10 years.

Key words: dry quenching coke oven, cooling zone, wear-resistant brick, wear amount

摘要:

为了提高干熄焦炉冷却段用耐磨砖的使用寿命,在原有B级莫来石砖的基础上,通过调整骨料粒度级配、加入SiC粉和红柱石微粉等研制了新型耐磨砖,并介绍了其在140 t·h-1干熄焦炉上的实际应用。结果表明:新型耐磨砖的耐压强度为160 MPa,磨损量仅为1.92 cm3,均优于原用B级莫来石砖的 。在140 t·h-1干熄焦炉冷却段使用7 a,炉衬表面仍然光洁平整,侵蚀量较小;预计该冷却段炉衬能使用10 a以上。