Abstract: In response to the problem of abnormally high temperatures at multiple points in the outlet pipeline of the mixing chamber of a hot blast stove in a certain iron plant,samples were selected from the residual lining after dismantling the mixing chamber.The chemical composition,microstructure,phase composition,thermal expansion and thermal shock resistance of the lining material were analyzed.The results show that the lining material adopts corundum castables,which have high strength and good wear resistance,and can effectively resist hot air erosion and CO corrosion damage.However,it has poor thermal shock resistance,and exhibits significant thermal expansion at high temperatures,leading to large internal thermal stresses.These stresses cause cracks to form within the material,which in turn allow the high-temperature and high-pressure hot blast to leak,resulting in an increase in the steel shell temperature.The measures taken are as follows:changing the corundum castables to corundum-mullite castables;when the mixing chamber is constructed with layered casting,the upper layer of castables must be cast before the initial setting of the lower layer of castables to ensure better fusion between the two layers of castables;and the three-way junction part can be changed from combined bricks to integral corundum-mullite castables.After the improvement,the surface temperature of the tube shell has dropped to normal and remains stable,the repair effect is good,and the service life is extended by about 5 years.

Key words: hot blast stoves, mixing chambers, corundum castables, thermal shock resistance, thermal expansion performance

摘要: 针对某铁厂热风炉混风室出口管道多处温度偏高的问题,对混风室拆除后的残衬进行取样,分析其化学组成、显微结构、物相组成、热膨胀性能及抗热震性。结果表明:衬体采用的是刚玉质浇注料,强度较高,耐磨性较好,能有效抵抗热风冲刷和CO侵蚀破坏,但抗热震性差,而且在高温下出现较大的热膨胀,内部出现了较大的热应力,使材料内部产生了裂纹,进而高温高压热风的窜漏造成钢壳温度上升。采取的措施有:由刚玉质浇注料改为刚玉-莫来石质浇注料;混风室施工分层浇注时,一定要在下层浇注料初凝之前浇注上层浇注料,保证两层间浇注料更好地融合;三岔口部位可由组合砖改为整体浇注刚玉-莫来石质浇注料。改进后,管壳表面温度已降至正常并稳定,修复效果较好,延长使用寿命5 a左右。

关键词: 热风炉, 混风室, 刚玉质浇注料, 抗热震性, 热膨胀性能