Corrosion of MgO-C bricks in carbonization electric furnace
Huang Jiaxu, Qi Jianling, Lyu Xueming, Liu Yadong
First author’s address:State Key Laboratory of Comprehensive Utilization of Vanadium and Titanium Resources Panzhihua Iron and Steel Research Institute Co.,Ltd.,Pangang Group,Panzhihua 617000,Sichuan,China
[1] 杨宇,梁精龙,李慧,等.攀钢含钛高炉渣资源化再利用进展[J].矿产综合利用,2018(2):12-15. [2] WANG D S,HOU Y Q,YE E D,et al.Adsorption behavior of Cl2 on TiC0.89O0.11(001) surface based on the first principle calculation[J].Surface Science,2024,750:122577. [3] WANG J X,YUE D,WEN L Y,et al.Experimental characterization of chemical mineral composition and morphology of titanium in carbonized slag particles[J].Journal of Materials Research and Technology,2025,34:1571-1581. [4] WANG D S,LV X M,HOU Y Q.Postmortem analysis of MgO-C bricks used in smelting furnace for fabricating TiC-bearing slag[J].Journal of Materials Research and Technology,2024,31:1171-1183. [5] 吕学明,郭文明,黄家旭,等.含钛高炉渣高温碳化过程出渣口耐材侵蚀研究[J].轻金属,2022(6):45-49. [6] 高伟,刘朝阳,马北越,等.钒钛磁铁矿熔渣与耐火材料间的相互作用[J].耐火材料,2023,57(4):365-368. [7] 毕万利,张玲,田琳,等.改性石墨对镁碳砖性能的影响[J].耐火材料,2011,45(3):184-186.