Refractories ›› 2021, Vol. 55 ›› Issue (1): 77-80.DOI: 10.3969/j.issn.1001-1935.2021.01.017

Previous Articles     Next Articles

Effect of four molten salts on synthesis of hercynite powder by molten salt method

Si Chaowei(), Lang Jiefu, You Jiegang(), Tan Wendong, She Yiming   

  1. School of Materials and Metallurgy,University of Science and Technology Liaoning,Anshan 114051,Liaoning,China
  • Received:2020-07-27 Online:2021-02-15 Published:2021-02-15
  • Contact: You Jiegang

四种熔盐对熔盐法合成铁铝尖晶石粉的影响

司超伟(), 郎杰夫, 游杰刚(), 谭文东, 佘以明   

  1. 辽宁科技大学 材料与冶金学院 辽宁鞍山 114051
  • 通讯作者: 游杰刚
  • 作者简介:司超伟:男,1995年生,硕士研究生。E-mail: scw_gongyong@163.com
  • 基金资助:
    辽宁省教育厅重点基金资助项目(2017LNZD06)

Abstract:

Hercynite powders were prepared using Fe2O3,Al2O3 and graphite powder as the raw materials,NaCl,KCl,NaCl-KCl and NaCl-Na2CO3 as the molten salt medium,fired at 1 000 ℃ for 3 h in high-purity nitrogen atmosphere by the molten salt method.The synthetic hercynite powders were analyzed by XRD,SEM-EDS and in terms of the particle size.The results show that hercynite is not formed using NaCl-Na2CO3 as the molten salt medium,because Na2CO3 reacts with Al2O3 to form Na2Al2O4 at a temperature above the melting point of Na2CO3 (851 ℃);high-purity hercynite can be synthesized using NaCl,KCl or NaCl-KCl as the molten salt medium;when NaCl-KCl is used as the molten salt medium,the average particle size of the hercynite is larger,and the particle distribution is more uniform compared with the one using NaCl or KCl.

Key words: molten salt method, hercynite, sodium chloride, potassium chloride, sodium carbonate

摘要:

以Fe2O3粉、Al2O3粉和石墨粉为主要原料,分别以NaCl、KCl、NaCl-KCl和NaCl-Na2CO3为熔盐介质,采用熔盐法在1 000 ℃高纯氮气气氛中保温3 h合成铁铝尖晶石粉,然后对合成铁铝尖晶石粉进行XRD、SEM-EDS和粒度分析。结果表明:以NaCl-Na2CO3作为熔盐介质未能合成出铁铝尖晶石,因为Na2CO3与Al2O3在Na2CO3熔点(851 ℃)以上温度反应生成了Na2Al2O4。以NaCl、 KCl和NaCl-KCl作为熔盐介质均能合成出纯度较高的铁铝尖晶石,并且在NaCl-KCl熔盐介质中合成的铁铝尖晶石的平均粒度比在KCl和NaCl熔盐介质中合成的铁铝尖晶石的大,粒度分布也更均匀。

关键词: 熔盐法, 铁铝尖晶石, NaCl, KCl, Na2CO3

CLC Number: