[1] 康国卫.六铝酸钙多孔材料的制备及其性能研究[D].郑州:郑州大学,2022. [2] 王长宝.六铝酸钙轻质耐火材料的研究[D].武汉:武汉科技大学,2008. [3] 田朋丹,王刚,杜鹏辉,等.聚丙烯纤维对刚玉-六铝酸钙浇注料抗热震性能的影响[J].耐火材料,2024,58(3):208-212. [4] 徐国涛,王志强,秦世民,等.新一代六铝酸钙质浇注料的研制与应用[J].耐火材料,2024,58(1):53-56. [5] 康国卫,刘苗伟,杨亚峰,等.熔盐造孔法制备六铝酸钙多孔材料[J].耐火材料,2021,55(5):448-451+455. [6] 范沐旭,侯晓静,冯志源,等.耐火材料抗碱蒸气侵蚀性研究[J].耐火材料,2021,55(4):296-301. [7] YANG H Z,LUO W,XIA Y F,et al.Convenient preparation of calcium hexaluminate based castables with low thermal conductivity and sufficient strength[J].International Journal of Applied Ceramic Technology,2024,21(4):2818-2823. [8] 李有奇,李亚伟,金胜利,等.六铝酸钙材料的合成及其显微结构研究[J].耐火材料,2004,38(5):318-323. [9] 曾春燕,刘艳改,徐友果,等.保温时间对合成轻质耐高温六铝酸钙材料性能的影响[J].人工晶体学报,2013,42(6):1199-1202+1207. [10] LI M H,LI Y B,OUYANG D G,et al.Effects of alumina bubble addition on the properties of mullite castables[J].Journal of Alloys and Compounds,2018,735:327-337. [11] LI X X,YAN L W,ZHANG Y B,et al.Lightweight porous silica ceramics with ultra-low thermal conductivity and enhanced compressive strength[J].Ceramics International,2022,48(7):9788-9796. [12] FANG B,ZHU B,LI X,et al.Pore size distribution and its quantitative relationship with strength of corundum based castables[J].China’s Refractories,2010,19(4):16-20. |