Refractories ›› 2026, Vol. 60 ›› Issue (2): 136-140.DOI: 10.3969/j.issn.1001-1935.2026.02.009

Previous Articles     Next Articles

Effect of Fe2O3 on performance of magnesia water-based gunning mix for converter large area

Xiao Yangwu, Ma Xiaoyi, Xiong Jiquan, Zhang Xiaocun, Nie Jianhua, Liang Yonghe, Ju Maoqi, Sun Huidong   

  1. First author’s address:Ironmaking Division,Shougang Shuigang Iron & Steel (Group) Co.,Ltd.,Liupanshui 553028,Guizhou,China
  • Received:2025-07-01 Online:2026-04-15 Published:2026-04-15

Fe2O3对转炉用镁质水系大面料性能的影响

肖扬武1), 马骁一2), 熊继全2), 张晓存3), 聂建华3), 梁永和3), 鞠茂奇2,3), 孙惠东2)   

  1. 1)首钢水钢钢铁(集团)有限责任公司 炼铁事业部 贵州六盘水 553028
    2)中冶武汉冶金建筑研究院有限公司 湖北武汉 430081
    3)武汉科技大学 先进耐火材料全国重点实验室 湖北武汉 430081
  • 作者简介:肖扬武:男,1974年生,高级工程师。E-mail:798615212@qq.com
  • 基金资助:
    国家自然科学基金联合基金重点项目(U21A2058);中国五矿集团有限公司青年科技基金(2024QNJJA05)。

Abstract: To improve the performance of water-based gunning mix for converter large area and prolong the service life of converters,magnesia water-based gunning mix was prepared with fused magnesia and silica fume as main raw materials.The effects of the sintering aid Fe2O3 additions (0,1%,2%,and 3%,by mass) on the properties of the gunning mix were studied,and its action mechanism in the gunning mix was explored.The results show that:(1)the introduction of Fe2O3 into the water-based gunning mix promotes the formation of MgFe2O4,which has a similar structure to MgAl2O4;and a continuous Mg(Fe,Al)2O4 solid solution forms between them,inducing lattice distortion,accelerating ion diffusion rate during the reaction,and promoting sample sintering;(2)Fe2O3 reacts with SiO2 in the sample to form FeO-SiO2,which is present as a liquid phase at 1 500 ℃,improving the sintering process,strengthening the bonding between particles and matrix,and promoting sample densification;(3)owing to the improved sintering performance,the cold physical properties of the samples are improved and the sintering time is shortened;however,excessive Fe2O3 leads to a large linear expansion rate of the sample,resulting in a loose structure.Therefore,the optimal addition of Fe2O3 is 2%.

Key words: gunning mix, Fe2O3, cold physical properties, sintering properties

摘要: 为了改善水系大面料的性能,提高转炉的使用寿命,以电熔镁砂和二氧化硅微粉等为主要原料制备了镁质水系大面料。研究了烧结助剂Fe2O3添加量(加入质量分数分别为0、1%、2%、3%)对大面料性能的影响并探明其在大面料体系中的作用机制。结果表明:1)在水系大面料中引入Fe2O3促进了MgFe2O4的形成,其与MgAl2O4结构相似,两者可形成Mg(Fe,Al)2O4连续固溶体,引起晶格畸变,加快反应中离子的扩散速率,促进试样烧结;2)Fe2O3的加入在试样中与SiO2生成FeO-SiO2系硅酸盐,其在1 500 ℃时呈液相,改善烧结过程,加强颗粒与基质间的结合,促进试样致密化;3)由于烧结性能提高,试样的常温物理性能得到改善,烧结时间缩短,但Fe2O3加入量过多,试样的线膨胀率较大,导致试样结构疏松,因此Fe2O3最佳的添加量为2%(w)。