Refractories ›› 2026, Vol. 60 ›› Issue (2): 156-160.DOI: 10.3969/j.issn.1001-1935.2026.02.013

Previous Articles     Next Articles

Effect of fluxes on properties of gangue-based foamed ceramics

Zhang Xiangfei, Lou Guanghui, Zhang Meng-zhen, Li Jing, Zhang Wanyu, Zhang Yisheng, Sun Maoze   

  1. First author’s address:Henan Building Materials Research and Design Institute Co.,Ltd.,Zhengzhou 450002,Henan,China
  • Received:2025-03-29 Online:2026-04-15 Published:2026-04-15

助熔剂对煤矸石基发泡陶瓷性能的影响

张祥飞1,2,3), 娄广辉1,2), 张梦真1), 李静1), 张碗玉1), 张艺升1), 孙茂泽4)   

  1. 1)河南建筑材料研究设计院有限责任公司 河南郑州 450002
    2)河南省科学院 河南郑州 450000
    3)河南师范大学 材料科学与工程学院 河南新乡 453007
    4)新乡城发中兴环保科技有限公司 河南新乡 453200
  • 作者简介:张祥飞:男,1997年生,硕士研究生。E-mail:jasonleap@163.com
  • 基金资助:
    河南省科学院高水平成果奖励与培育项目(242209024,20252209001);河南省科学院省级创新平台提升项目(20251009002)。

Abstract: To realize the resource utilization of solid waste gangue and develop high-performance foamed ceramics,gangue-based foamed ceramics were prepared using gangue as the primary raw material and SiC as the foaming agent,with Na2B4O7,Na2CO3,H3BO3 and Na2SiO3·9H2O as the fluxes,respectively,heat treating at 1 180 ℃ for 30 min.Firstly,the effect of flux types on the properties of the foamed ceramics was investigated,and Na2CO3 was identified as the optimal flux.Subsequently,the influence of the Na2CO3 additions (0,5%,10%,15%,and 20%,by mass) on the properties of the ceramics was further studied.The results indicate that the introduction of fluxes enables the preparation of gangue-based foamed ceramics at a low heat treatment temperature of 1 180 ℃.The foamed ceramic with 15% Na2CO3 exhibits the best overall properties:bulk density of 0.29 g·cm-3,compressive strength of 6.12 MPa,and apparent porosity of 84.3%.

Key words: gangue, foamed ceramics, fluxes, SiC

摘要: 为资源化利用煤矸石固体废弃物,开发高性能发泡陶瓷材料,以煤矸石为主要原料,SiC为发泡剂,分别采用Na2B4O7、Na2CO3、H3BO3和Na2SiO3·9H2O作为助熔剂,经1 180 ℃保温30 min热处理制备煤矸石基发泡陶瓷。先探讨助熔剂种类对发泡陶瓷性能的影响,确定最优助溶剂为Na2CO3,再进一步研究Na2CO3添加量(质量分数分别为0、5%、10%、15%和20%)对发泡陶瓷性能的影响。结果表明:助熔剂的引入使得低热处理温度1 180 ℃下制备煤矸石基发泡陶瓷成为可能,且添加15%(w)Na2CO3作为助熔剂的煤矸石基发泡陶瓷综合性能最佳,其体积密度为0.29 g·cm-3,压缩强度为6.12 MPa,显气孔率为84.3%。

关键词: 煤矸石, 发泡陶瓷, 助熔剂, SiC

CLC Number: