Refractories ›› 2026, Vol. 60 ›› Issue (2): 167-172.DOI: 10.3969/j.issn.1001-1935.2026.02.015

Previous Articles     Next Articles

Progress in chemical impurity removal technologies for magnesite and its tailings

Lan Zhipeng, Yuan Xiao-zhou, Yang Xin, Yang Huan, Wang Qianqian, Zhao Guangyi, Li Guangming, Ma Beiyue   

  1. First author’s address:Key Laboratory of Ecological Metallurgy of Polymetallic Symbiotic Minerals,Ministry of Education,School of Metallurgy,Northeastern University,Shenyang 110819,Liaoning,China
  • Received:2025-06-04 Online:2026-04-15 Published:2026-04-15

菱镁矿及其尾矿化学法除杂技术进展

兰志鹏1), 苑小舟1), 杨欣1), 杨欢1), 王千千1), 赵广义2), 李广明3), 马北越1)   

  1. 1)东北大学冶金学院 多金属共生矿生态化冶金教育部重点实验室 辽宁沈阳 110819
    2)辽宁科之镁新材料研究有限公司 辽宁沈阳 110000
    3)大石桥市美尔镁制品有限公司 辽宁营口 115100
  • 作者简介:兰志鹏:男,2000年生,硕士研究生。E-mail:1286485330@qq.com
  • 基金资助:
    国家自然科学基金资助项目(U20A20239)。

Abstract: It is difficult for physical mineral processing to treat magnesite with fine dissemination and isomorphic impurities,resulting in resource waste.Therefore,the present situation of chemical impurity removal technologies for magnesite and its tailings was summarized,including the widely used ammonium salt method and acid leaching method,the carbonization method based on specific reactions,the simple and environmentally friendly hydration method,and the chlorination roasting method with high purification efficiency.It was pointed out that the impurity removal of low grade magnesite should focus on the research and development of technologies and green leaching agents as well as the construction of a full industrial chain model.

Key words: magnesite, tailings, ammonium salt method, carbonization method, acid leaching method, hydration method, chlorination roasting method

摘要: 物理选矿法难以处理微细嵌布且杂质呈类质同象的菱镁矿,造成资源的浪费。为此,概述了菱镁矿及其尾矿化学法除杂技术现状,包括应用广泛的铵盐法、酸浸法,基于特定反应的碳化法,工艺简洁环保的水化法,提纯效率高的氯化焙烧法,指出低品位菱镁矿除杂应聚焦技术研发、绿色浸取剂研发及全产业链模式构建的发展方向。

关键词: 菱镁矿, 尾矿, 铵盐法, 碳化法, 酸浸法, 水化法, 氯化焙烧法

CLC Number: