| [1] |
Li Ying, Wang Di, Zhao Li, Yin Yicheng, Jia Quanli.
Effect of graphite type on properties of Al2O3-MgO castables
[J]. Refractories, 2024, 58(4): 323-328.
|
| [2] |
Tian Pengdan, Wang Gang, Du Penghui, Feng Haixia, Wang Laiwen, Pan Yuanshuai.
Effects of polypropylene fibers on thermal shock resistance of corundum-calcium hexaaluminate castables
[J]. Refractories, 2024, 58(3): 208-212.
|
| [3] |
Shao Rongdan, Ju Maoqi, Cheng Shui-ming, Xia Changyong, Li Xuzhi, Zhang Han, Shan Jiangbo.
Effect of boron oxide on mechanical properties of Al2O3-SiC-C castables
[J]. Refractories, 2024, 58(3): 230-233.
|
| [4] |
Ju Maoqi, Ma Xiaoyi, Cheng Shuiming, Xia Changyong, Wei Jianxiu, Zhang Xiaocun, Shan Jiangbo, Gao Dongsheng.
Effects of spent iron trough castable addition on properties of Al2O3-SiC-C castables
[J]. Refractories, 2024, 58(3): 238-241.
|
| [5] |
Wang Yongxin, Gao Yabo, Fang Yaohua, Li Yage, Huang Zhong, Zhang Haijun.
Research progress of SiO2,Al2O3,and MgO micropowder binders for refractory castables
[J]. Refractories, 2024, 58(2): 167-173.
|
| [6] |
Yang Zongyuan, Wang Jing-ran, Wang Tong, Zhang Jinhua, Han Bingqiang, Ni Yue'e, Ke Changming.
Corrosion behavior of slags with different basicities to corundum spinel castables
[J]. Refractories, 2024, 58(1): 13-18.
|
| [7] |
Xu Guotao, Wang Zhi-qiang, Qin Shimin, Liu Li, Zhang Honglei, Zhang Yanwen, Zhou Wangzhi.
Development and application of new generation calcium hexaaluminate castables
[J]. Refractories, 2024, 58(1): 53-56.
|
| [8] |
Xia Yuting, Yang Wenbo, Rao Yutong, Nie Ruishan, Yao Yuan.
Composition optimization and performance enhancement of lightweight and high-strength mullite castables
[J]. Refractories, 2024, 58(1): 72-75.
|
| [9] |
Liu Xuexin, Zhang Jinhua, Chen Xinming, Wang Jingran, Yang Zongyuan, Han Bingqiang, Ke Changming.
Preparation of corundum-spinel castables using microporous corundum-spinel aggregates to replace corundum aggregates
[J]. Refractories, 2023, 57(6): 514-517.
|
| [10] |
Ding Yuhang, Liu Huiyong, Cong Peiyuan, Cai Wei, Xiang Bing, Xia Changyong.
Effect of aluminate cement on structure and properties of silica sol bonded corundum castables
[J]. Refractories, 2023, 57(6): 523-527.
|
| [11] |
Zhao Zongqiang, Zhang Hongrui, Chen Liugang.
Properties comparison of reactive MgO and calcium aluminate cement bonded corundum-spinel castables
[J]. Refractories, 2023, 57(6): 528-530.
|
| [12] |
Lyu Siwei, Li Minghui, Ni Wei, Tong Shengli, Chen Ruoyu, Li Saisai, Li Canhua.
Effect of spodumene particle size on properties of Al2O3-SiC-C castables
[J]. Refractories, 2023, 57(4): 337-342.
|
| [13] |
Long Tu, Gu Huazhi, Zhang Meijie, Huang Ao, Qiu Wendong.
Effects of ferrotitanium slag addition on properties of Al2O3-SiC-C iron trough castables
[J]. Refractories, 2023, 57(4): 351-355.
|
| [14] |
Qin Hongbin, Jin Feng, Tang Shiming, Zhou Huijun, Li Hongxia, Shi Shubing, Zhang Sanhua, Cheng Li, Hui Xianlei.
Effect of calcium dialuminate addition on properties of corundum castables
[J]. Refractories, 2023, 57(3): 189-193.
|
| [15] |
Zan Wenyu, Ma Beiyue, Wang Yuqing, Jiang Zhifeng.
Preparation of lightweight alumina-silica castables by replacing open-pore perlite aggregates with coal gangue ceramsite
[J]. Refractories, 2023, 57(3): 205-209.
|