Sun Honggang, Li Hongxia, Si Yaochen, Du Yihao, Zhao Shixian, Shang Xinlian, Xia Miao   

  1. First author's address: State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2023-07-11 Online:2023-10-15 Published:2023-10-26

热处理温度对SiC-MgAl2O4-Al复合材料性能的影响

孙红刚, 李红霞, 司瑶晨, 杜一昊, 赵世贤, 尚心莲, 夏淼   

  1. 中钢集团洛阳耐火材料研究院有限公司 先进耐火材料国家重点实验室 河南洛阳 471039
  • 作者简介:孙红刚:男,1979年生,博士,正高级工程师。E-mail:sunhonggang@hotmail.com
  • 基金资助:
    国家自然科学基金项目(U21A2059、52072346)。

Abstract: In order to improve the mechanical properties of SiC-MgAl2O4 composites for coal gasifiers,SiC-MgAl2O4-Al composites were prepared by heat treatment in the nitrogen atmosphere using SiC particles (≤ 2.5 mm),MgAl2O4 fine powder (≤90 μm),α-Al2O3 micro-powder(d50≈5 μm) and aluminum powder (≤74 μm) as the main raw materials.The effects of different heat treatment temperatures from 200 ℃ to 1 600 ℃ on the microstructure,phase composition and mechanical properties of the composites were analyzed.The results show that:(1)when the heat treatment temperature is higher than 1 000 ℃,Al in the composites gradually forms Al-O-C-N whiskers,which can significantly improve the mechanical properties of the composites;(2)the cold and hot modulus of rupture increases with the increasing content and size of Al-O-C-N whiskers in the composites.The phase composition,content,and morphology of the Al-O-C-N whiskers can be controlled by adjusting the heat treatment temperature,thereby achieving the control of the phase composition and microstructure,and improving the mechanical properties of the composites.

Key words: SiC-MgAl2O4 composites, aluminum, microstructure, hot modulus of rupture, heat treatment temperature

摘要: 为提高煤气化炉用碳化硅-尖晶石复合材料的力学性能,以SiC颗粒(≤2.5 mm)、尖晶石细粉(≤90 μm)、α-Al2O3微粉(d50≈5 μm)和金属Al粉(≤74 μm)为主要原料,在氮气气氛中进行热处理,制备了SiC-MgAl2O4-Al复合材料。分析了200~1 600 ℃不同热处理温度对复合材料显微结构、物相组成和力学性能的影响。结果表明:1)当热处理温度大于1 000 ℃时,复合材料中的Al开始逐渐反应生成Al-O-C-N晶须,可显著提升材料的力学性能。2)常温和热态抗折强度随着复合材料内Al-O-C-N晶须含量的增多和尺寸的增大而提高。通过调整热处理温度可调控材料内Al-O-C-N晶须的物相组成、含量和形貌等,从而实现对复合材料物相组成与显微结构的调控,提升材料的力学性能。

关键词: 碳化硅-尖晶石复合材料, 金属Al, 显微结构, 热态抗折强度, 热处理温度