Refractories ›› 2024, Vol. 58 ›› Issue (2): 167-173.DOI: 10.3969/j.issn.1001-1935.2024.02.014

Previous Articles     Next Articles

Research progress of SiO2,Al2O3,and MgO micropowder binders for refractory castables

Wang Yongxin, Gao Yabo, Fang Yaohua, Li Yage, Huang Zhong, Zhang Haijun   

  1. First author's address: The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2023-07-22 Online:2024-04-15 Published:2024-04-24

耐火浇注料用SiO2、Al2O3和MgO微粉结合剂研究进展

王永新, 高亚博, 方要华, 李亚格, 黄仲, 张海军   

  1. 武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
  • 作者简介:王永新:男,1999年生,硕士研究生。 E-mail:254896083@qq.com
  • 基金资助:
    国家自然科学基金(52202025;52272021;52232002)。

Abstract: Binders are an important part of refractory castables,which not only provide early working performance and mechanical strength for refractory castables,but also affect their high-temperature performance.Hence,the research progress and problems of SiO2,Al2O3 and MgO micropowder binders for refractory castables in recent years were summarized in order to promote the future research and application.

Key words: refractory castables, micropowder, binder, mechanical property

摘要: 结合剂是耐火浇注料的重要组成部分,为耐火浇注料提供了早期作业性能和力学强度,并可影响耐火浇注料在高温下的使用性能。对近年来耐火浇注料用SiO2、Al2O3以及MgO微粉结合剂的研究进展及仍存在的一些问题作出了总结,期望为其进一步研究和更好的应用起到积极的推进作用。

关键词: 耐火浇注料, 微粉, 结合剂, 力学性能