Refractories ›› 2024, Vol. 58 ›› Issue (4): 357-361.DOI: 10.3969/j.issn.1001-1935.2024.04.016

Previous Articles     Next Articles

Development status of fused magnesia in southern Liaoning

You Jiegang, Zhao Xin, Qian Guohua, Zhang Xiao-fang, Zhang Guodong, Ma Beiyue   

  1. First author's address: College of Materials and Metallurgy,University of Science and Technology Liaoning,Anshan 110051,Liaoning,China
  • Received:2023-12-01 Online:2024-08-15 Published:2024-08-21

辽南地区电熔镁砂的发展现状

游杰刚1), 赵鑫1), 钱国华2), 张小芳1), 张国栋3), 马北越4)   

  1. 1)辽宁科技大学 材料与冶金学院 辽宁鞍山 110051
    2)泰州市旺鑫耐火材料有限公司 江苏泰州 225300
    3)辽宁省非金属矿工业协会 辽宁沈阳 110870
    4)东北大学 冶金学院 辽宁沈阳 110809
  • 作者简介:游杰刚:男,1975年生,博士,教授。E-mail:youjiegang@163.com
  • 基金资助:
    国家自然科学基金资助项目(U20A20239)。

Abstract: Fused magnesia is a main irreplaceable raw material of magnesia-carbon bricks for the linings of steelmaking converters,steelmaking electric furnaces and refining ladle slag lines,which has a production capacity of 4 million tons in southern Liaoning.However,due to its downstream market,production raw materials,as well as production technology and equipment,problems for the fused magnesia production exist such as the imbalance of supply and demand,high energy consumption and large fluctuation of product quality.Therefore,the status and changes of fused magnesia in southern Liaoning in recent years were expounded.The future development trend of fused magnesia was pointed out.

Key words: fused magnesia, single product energy consumption, magnesite, kiln

摘要: 电熔镁砂主要作为炼钢转炉、精炼钢包渣线以及炼钢电炉炉衬镁碳砖不可取代的原料,已在辽南地区形成了400万t以上的生产能力。但由于电熔镁砂下游市场、生产原料、生产技术和装备等原因,电熔镁砂生产存在供需不平衡、能耗高、产品质量波动大等问题。为此,阐述了近年来辽南地区电熔镁砂的现状与变化,并指出了电熔镁砂未来的发展趋势。

关键词: 电熔镁砂, 单品能耗, 菱镁矿, 窑炉