Refractories ›› 2024, Vol. 58 ›› Issue (1): 80-86.DOI: 10.3969/j.issn.1001-1935.2024.01.017

Previous Articles     Next Articles

Application progress of mullite composite refractories

Zhang Wei, Wang Jingyang   

  1. First author's address: Shenyang National Laboratory for Materials Science,Institute of Metal Research,Chinese Academy of Sciences,Shenyang 110016,Liaoning,China
  • Received:2023-04-07 Online:2024-02-15 Published:2024-02-28

莫来石复合耐火材料的应用进展

张巍, 王京阳   

  1. 中国科学院金属研究所 沈阳材料科学国家研究中心 辽宁沈阳 110016
  • 作者简介:张巍:男,1982年生,博士,副研究员。E-mail:cnzhangwei2008@126.com
  • 基金资助:
    中国科学院金属研究所自主部署项目(E255L401)。

Abstract: Mullite has a high melting point,high hardness,and good thermal shock resistance,corrosion resistance and hot mechanical properties.Mullite raw materials are mostly synthesized by the sintering method and electric melting method.The research and application progress of mullite composite refractories produced from mullite in the fields such as ceramics,metallurgy,aerospace,military industry,cement and glass were reviewed.The future developing of mullite in refractories was prospected.

Key words: mullite, refractories, metallurgy, kiln furniture, aerospace, military industry

摘要: 莫来石具有较高的熔点,较大的硬度,良好的抗热震性、抗侵蚀性、高温力学性能等。莫来石原料多通过烧结法和电熔法合成。综述了以莫来石为原料制备的莫来石复合耐火材料在陶瓷、冶金、航天、军工、水泥、玻璃等领域的研究与应用进展,指出了莫来石在耐火材料应用中的发展趋势。

关键词: 莫来石, 耐火材料, 冶金, 窑具, 航天, 军工