Refractories ›› 2021, Vol. 55 ›› Issue (1): 89-92.DOI: 10.3969/j.issn.1001-1935.2021.01.019
Zhang Yucui1)(
), Cui Qingyang1), Gao Song1), Jiao Zhiyu1), Hu Yancang2)
Received:2020-07-01
Online:2021-02-15
Published:2021-02-15
张宇翠1)(
), 崔庆阳1), 高耸1), 焦智宇1), 胡艳仓2)
作者简介:张宇翠:女,1987年生,硕士,工程师。E-mail: zhangxiaocui- 1987@163.com
CLC Number:
Zhang Yucui, Cui Qingyang, Gao Song, Jiao Zhiyu, Hu Yancang. Research progress of application of additives in MgO-MA materials[J]. Refractories, 2021, 55(1): 89-92.
张宇翠, 崔庆阳, 高耸, 焦智宇, 胡艳仓. 添加剂在MgO-MA质材料中应用的研究进展[J]. 耐火材料, 2021, 55(1): 89-92.
Add to citation manager EndNote|Ris|BibTeX
URL: http://www.nhcl.cn/EN/10.3969/j.issn.1001-1935.2021.01.019
| [1] | 饶东生. 硅酸盐物理化学[M]. 北京: 冶金工业出版社, 1991: 21-36. |
| [2] | 李建平, 谢玉玲. 镁铝尖晶石的合成及其工业应用[J]. 非金属矿, 1996(4):24-27. |
| [3] |
GANESH I, BHATTACHARJEE S, SAHA B P, et al. An efficient MgAl2O4 spinel additive for improved slag erosion and penetration resistance of high-Al2O3 and MgO-C refractories[J]. Ceramics International, 2002,28(3):245-253.
DOI URL |
| [4] |
PARK C H, LEE B Y, OH D K, et al. Grain growth in sintered MgAl2O4 spinel[J]. Journal of Materials Science Letters, 1997,16(22):1841-1844.
DOI URL |
| [5] |
AKSEL C, KASAP F, RILEY F L, et al. Mechanical properties of magnesia-spinel composites[J]. Journal of the European Ceramic Society, 2002,22(5):745-754.
DOI URL |
| [6] | MASCHIOR D, FABBRI B, FIORI C. Industrial applications of refractories containing magnesium aluminate spinel[J]. Industrial Ceramics, 1988,8(2):121-126. |
| [7] | 桂明玺,译. 水泥回转窑烧成带用无铬砖的开发[J]. 国外耐火材料, 2002(5):18-21. |
| [8] | 李静捷. RH浸渍管用方镁石-尖晶石质耐火材料研究[D]. 武汉:武汉科技大学, 2016. |
| [9] | TOKUNAGA K, KOZUKA H, HONDA T, et al. Further improvements in high temperature strength,coating adherence,and corrosion resistance of magnesia-spinel bricks for rotary cemem kiln[C]// Proc of UNITECR’1991,Aachen,Germany, 1991: 431-435. |
| [10] |
GHOSH A, DAS S K, BISWAS J R, et al. The effect of ZnO addition on the densification and properties of magnesium aluminate spinels[J]. Ceramics International, 2000,26(6):605-608.
DOI URL |
| [11] | 赵中令. RH炉下部槽用无铬不烧砖的研究[D]. 鞍山:辽宁科技大学, 2015. |
| [12] | BAIKY H. Sintering of MgAl2O4 spinel and its characteristics[J]. Yoop Hikoechi, 1985,22(6):29-36. |
| [13] | 李国军, 黄校先, 郭景坤. Al2O3基金属陶瓷的研究现状[J]. 材料导报, 2000,14(9):22-24. |
| [14] |
SARINA B, KAI T, ANNE K, et al. Wettability of aluminum on alumina[J]. Metallurgical and Materials Transactions B, 2011,42(6):1358-1366.
DOI URL |
| [15] |
HONG Y, LI Y, TONG S H, et al. Effect of the addition of Al powder on the microstructure and phase constitution of magnesia-spinel composites sintered at 1 800 ℃ in N2[J]. Key Engineering Materials, 2016,697:345-349.
DOI URL |
| [16] | 何俊鹏. 炉外精炼用方镁石-尖晶石质耐火材料研究[D]. 武汉:武汉科技大学, 2013. |
| [17] | 郭海珠, 余森. 实用耐火原料手册[M]. 北京: 中国建材工业出版社, 2000: 319-333. |
| [18] | 桂舜, 王周福, 王玺堂, 等. 铝、硅添加对方镁石-铝镁尖晶石质免烧耐火材料性能的影响[J]. 武汉科技大学学报, 2019,42(4):272-276. |
| [19] |
TONG S H, LI Y, ZHAO J Z, et al. Effect of Al addition on creep resistance of MgO-Al2O3 composite for sliding plate at 1 400 ℃[J]. Ceramics International, 2017,43(15):11610-11615.
DOI URL |
| [20] | 谢安宁. Al-MgAl2O4和Al-MgO-MgAl2O4体系中生成MgAlON的形貌[J]. 耐火材料, 2017,51(6):434-437. |
| [21] | 栾舰, 王春艳, 周大鹏, 等. 添加Al的MgO-MA材料的相组成和显微结构[C]// 第十二届全国不定形耐火材料学术会议和2013年耐火原料学术交流会论文集,洛阳, 2013: 212-213. |
| [22] | 岳卫东. 矾士基β-Sialon复合低碳铝碳滑板材料的研究[D]. 郑州:郑州大学, 2007. |
| [23] | 孙宇飞, 王雪梅, 王诚训, 等. 镁质和镁基复相耐火材料[M]. 北京: 冶金工业出版社, 2010: 205-212. |
| [24] |
SARKAR R, DAS S K, BANNERJEE G. Effect of additives on the densification of reaction sintered and presynjournaled spinels[J]. Ceramics International, 2003,29(1):55-59.
DOI URL |
| [25] | 刘东方, 马向东, 张志浩, 等. TiO2含量对镁铝尖晶石烧结性能的影响[J]. 硅酸盐通报, 2016,35(8):2481-2485. |
| [26] | 王守权. 添加氧化钛的尖晶石烧结性状[J]. 国外耐火材料, 2000(3):55-59. |
| [27] | YU J, HIRAGUSHI K. Sintering behaviour of spinel with added TiO2[J]. Taikabutsu Overseas 16, 1996,61(37):125-134. |
| [28] | 董计太. RH炉浸渍管用方镁石-镁铝尖晶石质耐火材料性能研究[D]. 鞍山:辽宁科技大学, 2016. |
| [29] | 董计太, 陈树江, 李国华, 等. 复合添加剂对RH炉浸渍管用MgO-MgO·Al2O3砖性能的影响[J]. 硅酸盐通报, 2015,34(7):2030-2035. |
| [30] | KAI T, ISAJI K. Improvement of magnesia-spinel brick for refining ladle[J]. Taikabutsu, 2011,53(9):521-526. |
| [31] | 樊余顺. 添加ZrO2对MgO-MgO·Al2O3系耐火材料的性能影响[J]. 江苏陶瓷, 2004,37(2):39-40. |
| [32] |
RASIM C, CEMAIL A. Improvements on the mechanical properties and thermal shock behaviors of MgO-spinel composite refractories by ZrO2 incorporation[J]. Ceramics International, 2012,38(2):995-1002.
DOI URL |
| [33] |
CEYLANTEKIN R, AKSEL C. Improvements on the corrosion behaviors of MgO-spinel composite refractories by addition of ZrSiO4[J]. Ceramics International, 2012,38(4):995-1002.
DOI URL |
| [34] |
SAHIN B, AKSEL C. Developments on the mechanical properties of MgO-MgAl2O4 composite refractories by ZrSiO4-3 mol% Y2O3 addition[J]. Journal of the European Ceramic Society, 2012,32(1):49-57.
DOI URL |
| [35] | 陈肇友. 从相图讨论MgO-CaO-ZrO2耐火材料抗炉外精炼渣与水泥的侵蚀[J]. 耐火材料, 2002,36(2):107-110. |
| [36] |
PAVLYUCHKOV D, SAVINYKH G, FABRICHNAYA O. Experimental investigation and thermodynamic modeling of the ZrO2-MgO-Al2O3 system[J]. Journal of the European Ceramic Society, 2014,34(5):1397-1408.
DOI URL |
| [37] |
HAYASKI H, SAITOU T, MARUYAMA N, et al. Thermal expansion coefficient of yttria stabilized zirconia for various yttria contents[J]. Solid State Ionics, 2004,176(5):613-619.
DOI URL |
| [38] |
AKSEL C, WARREN P D. Work of fracture and fracture surface energy of magnesia-spinel composites[J]. Compos Sci Technol, 2003,63(10):1433-1440.
DOI URL |
| [39] |
YAN M W, LI Y, YIN G X, et al. Synjournal and characterization of a MgO-MgAl2O4-ZrO2 composite with a continuous network microstructure[J]. Ceramics International, 2017,43(8):5914-5919.
DOI URL |
| [40] |
LAMPROPOULOU P G, KATAGAS C G. Effects of zirconium silicate and chromite addition on the microstructure and bulk density of magnesia-magnesium aluminate spinel-based refractory materials[J]. Ceramics International, 2007,34(5):1247-1252.
DOI URL |
| [41] |
SARKAR R, DAS S K, BANERJEE G. Effect of addition of Cr2O3 on the properties of reaction sintered MgO-Al2O3 spinels[J]. Journal of the European Ceramic Society, 2002,22(8):1243-1250.
DOI URL |
| [42] | 王诚训, 张义先. 镁铬铝系耐火材料[M]. 北京: 冶金工业出版社, 1995: 85-116. |
| [43] | 李红霞, 王金相. 水泥窑用碱性耐火材料无铬化的技术进展[J]. 中国水泥, 2004(10):79-82. |
| [44] | GAO S, YAN H, TONG S H, et al. Development and application of chromium-free magnesia spinel refractory used in rh refining furnace[C]// Proceedings of the 2018 International Conference on Refractories,Hang Zhou, 2018: 367-372. |
| [45] | SARKAR R., TRIPATHI H S, GHOSH A. Reaction sintering of different spinel composition in the presence of Y2O3[J]. Materials LeRers, 2004,58(16):2186-2191. |
| [46] |
LI J, LIU J H, LÜ X J, et al. Effect of Sc2O3 addition on densification and microstructure of different spinelized magnesium aluminate spinels[J]. Transactions of Nonferrous Metals Society of China, 2016,26(1):144-151.
DOI URL |
| [47] | 王周福, 徐自伟, 张保国, 等. 混合稀土氧化物对镁质耐火材料结构与性能的影响[J]. 稀有金属材料与工程, 2007,36(S2):373-375. |
| [48] | SHIMIZU K, HOKII T, ASANO K, et al. Chrome-free brick applied tolower vessel of RH degasser[C]// Proc of UNITECR’03,Osaka,Japan, 2003: 118-121. |
| [1] | Yao Luyan, Han Bingqiang, Zhang Jinhua, Ke Changming. Effect of Ti-Si-Fe alloy addition on structure and properties of Si3N4 bonded SiC refractories [J]. Refractories, 2024, 58(4): 277-283. |
| [2] | Jia Huan, Feng Xu, Yuan Hudie. Research progress of Ti3SiC2 matrix composites [J]. Refractories, 2024, 58(4): 362-368. |
| [3] | Wang Meng, Wen Shuhua, Yu Jingkun, Yuan Lei, Wen Tianpeng. Preparation of calcium zirconate materials by two-step sintering [J]. Refractories, 2024, 58(3): 204-207. |
| [4] | Liang Xiaocheng, Feng Yu, Liu Zhongfei, Luo Xudong, Huang Min, Wu Feng. Effect of pre-synthesized CaZrO3 on properties of magnesia-zirconia refractories [J]. Refractories, 2024, 58(3): 213-217. |
| [5] | Meng Hongtao, Ma Longbin, Liu Xin. Effect of pre-oxidation on oxidation resistance of nitrides bonded silicon carbide materials for coke ovens [J]. Refractories, 2024, 58(3): 242-245. |
| [6] | Zhou Yudong, Li Shipeng, Wang Wenwu, Zhang Yifan, Zhao Chenxiao. Research progress on preparation of high thermal conductivity silicon nitride ceramics [J]. Refractories, 2024, 58(3): 270-276. |
| [7] | Zhang Hui, Chai Qian, Zhang Hong, Wang Yixing, Hao Chenxi, Wang Xingyu. Effects of zirconia and lanthana co-doping on properties of porous cordierite ceramics [J]. Refractories, 2024, 58(2): 99-103. |
| [8] | Yang Dekai, Wang Zhou-fu, Liu Hao, Ma Yan, Wang Xitang, Zhou Jing. Preparation of soil polymers and their effects on properties of corundum castables [J]. Refractories, 2024, 58(2): 104-109. |
| [9] | Yao Wankai, Fang Binxiang, Li Xiangcheng, Chen Ping’an, Zhu Yingli, Zhu Boquan. Research progress on strengthening and toughening of boron carbide composite ceramics [J]. Refractories, 2023, 57(6): 531-537. |
| [10] | Shi Gan, Fan Muxu, Liu Xinyu. Effect of solid solution reaction on structure and properties of MA-Al2O3 materials [J]. Refractories, 2023, 57(5): 386-389. |
| [11] | Lu Yue, Liu Guoqi, Yang Wengang, Yan Pengfei, Ma Weikui, Li Hongxia. Effect of sintering agent on properties of calcium zirconate materials [J]. Refractories, 2023, 57(5): 407-411. |
| [12] | Hu Deng, Zhang Han, Huang Xuezhong, Liu Hongbo, Zhao Huizhong. Effect of CaO addition on properties of alumina-magnesia dry ramming mix for medium frequency furnaces [J]. Refractories, 2023, 57(4): 347-350. |
| [13] | Wang Jianbin, Wang Zhanmin, Feng Haixia, Liu Jun, Han Yihui, Pan Yuanshuai. Research progress on effect of raw material characteristics on sintering densification of magnesium aluminate spinel [J]. Refractories, 2023, 57(3): 259-264. |
| [14] | Zhang Yifan, Wang Qu, Wang Gang, Lu Keke, Zhang Qi. Effect of ZrO2 addition on lanthanum aluminate based high emissivity coating materials [J]. Refractories, 2023, 57(1): 6-9. |
| [15] | Guo Huishi, Chen Wenliang, Li Wenfeng, Yang Jialin, Qin Xiaomei, Gui Yanghai, Liu Yingfan. Effects of sintering temperatures on microstructure and properties of mullite porous ceramics [J]. Refractories, 2023, 57(1): 10-14. |
| Viewed | ||||||
|
Full text |
|
|||||
|
Abstract |
|
|||||