Preparation of TiN nanomaterials and their photothermal conversion applications
Cao Yunbo, Liang Feng, Wang Sen, He Jiangfeng, Wang Xiaohan, Hao Xian, Zhang Haijun
Refractories . 2021, (
3
): 244 -250 . DOI: 10.3969/j.issn.1001-1935.2021.03.015