Postmortem analysis of phosphate containing high chrome refractories in a coal water slurry gasifier
Sun Honggang, Li Hongxia, Geng Keming, Yan Shuangzhi, Du Yihao, Wang Han, Zhao Shixian
Refractories . 2021, (4): 277 -282 .  DOI: 10.3969/j.issn.1001-1935.2021.04.001