K 2CO 3 corrosion resistance of CA 6,MA or β-Al 2O 3 castables
Xu Yuanchao, Zhang Sanhua, Qin Hongbin, Xu Yingshun, Huang Zhilin
Refractories . 2022, (5): 412 -415 .  DOI: 10.3969/j.issn.1001-1935.2022.05.009