Effect of ferric nitrate loading mode on properties of Si
3
N
4
composite MgO-C refractories prepared by nitridation
Chen Yang, Deng Chengji, Ding Jun, Yu Chao, Lou Xiaoming
Refractories . 2022, (
6
): 477 -480 . DOI: 10.3969/j.issn.1001-1935.2022.06.004